盐-冻融作用下水泥乳化沥青混合料性能损伤规律研究

Study on the Performance Deterioration Law of Cement Emulsified Asphalt Mixtures under Salt-Freeze-Thaw Action

为明确寒冷及融雪盐环境下水泥乳化沥青混合料的耐久性衰减特征, 本文以水泥乳化沥青混合料为研究对象, 采用清水与15% NaCl溶液进行冻融循环处理, 系统分析不同冻融循环次数对其高温稳定性、低温抗裂性和水稳定性的影响。结果表明, 冻融循环会持续削弱水泥乳化沥青混合料的路用性能, 且盐溶液冻融作用下的损伤程度明显高于清水冻融作用。随着循环次数由1次增加至15次, 动稳定度、最大弯拉应变和劈裂强度比均出现不同程度下降, 说明水分迁移、冰胀压力、盐分侵蚀以及水泥水化产物与乳化沥青膜界面弱化共同加速了混合料内部结构损伤。研究结果可为水泥乳化沥青混合料在寒冷地区及融雪盐环境下的材料设计和耐久性评价提供参考。 

To clarify the durability degradation characteristics of cement emulsified asphalt mixtures under cold and de-icing salt environments, this study subjects cement emulsified asphalt mixtures to free-thaw cycles in both water and 15% NaCl solution, and systematically analyzes the effects of different freeze-thaw cycle counts on their high-temperature stability, low-temperature crack resistance, and water stability. The results show that freeze-thaw cycles continuously weaken the road performance of cement emulsified asphalt mixtures, and the degree of deterioration caused by salt-solution freeze-thaw is significantly higher than that caused by water freeze-thaw. As the cycle counts increase from 1 to 15, the dynamic stability, maximum flexural strain, and splitting strength ratio all decrease to varying degrees, indicating that moisture migration, ice expansion pressure, salt erosion, and the weakening of the interface between cement hydration products and the emulsified asphalt film collectively accelerate the internal structural deterioration of the mixtures. The findings can provide a reference for the material design and durability evaluation of cement emulsified asphalt mixtures in cold regions and under de-icing salt environments.